Nana Kwabena Adomako, Sanghoon Noh, Chang-Seok Oh, et al. Laser deposition additive manufacturing of 17-4PH stainless steel on Ti-6Al-4V using V interlayer[J]. Materials Research Letters, 2019, 7(7): 259-266.
DOI:
Nana Kwabena Adomako, Sanghoon Noh, Chang-Seok Oh, et al. Laser deposition additive manufacturing of 17-4PH stainless steel on Ti-6Al-4V using V interlayer[J]. Materials Research Letters, 2019, 7(7): 259-266.DOI: 10.1080/21663831.2019.1596989.
Laser deposition additive manufacturing of 17-4PH stainless steel on Ti-6Al-4V using V interlayer
additive manufacturing was used to obtain a strong joint (bonding strength 200 MPa) between stainless steel and Ti-6Al-4V using a V interlayer. The V interlayer applied via solid-state joining prevented the formation of brittle intermetallic phases more effectively than a V interlayer deposited by a liquid-state process. The microstructure and strength of the joint interface depended on the laser power and scan speed. The joint strength decreased with increasing annealing time
especially after 4 and 24 h
demonstrating the presence of the Fe-V-Cr σ-phase.