Improved fatigue properties of laser powder bed fusion of Al–4.74Mg–0.70Sc–0.32Zr alloy via hot isostatic pressing
Original Reports|更新时间:2026-08-19
|
Improved fatigue properties of laser powder bed fusion of Al–4.74Mg–0.70Sc–0.32Zr alloy via hot isostatic pressing
Improved fatigue properties of laser powder bed fusion of Al–4.74Mg–0.70Sc–0.32Zr alloy via hot isostatic pressing
材料研究快报(英文)2022年10卷第11期 页码:720-727
作者机构:
1. b Key Laboratory of Metal High Performance Additive Manufacturing and Innovative Design MIIT China Northwestern Polytechnical University
2. a State Key Laboratory of Solidification Processing Northwestern Polytechnical University Xi’an People’s Republic of China
3. b Key Laboratory of Metal High Performance Additive Manufacturing and Innovative Design MIIT China Northwestern Polytechnical University Xi'an People’s Republic of China
4. a State Key Laboratory of Solidification Processing Northwestern Polytechnical University
5. d Sichuan Aerospace Chuannan Initiating Explosive Technology Limited
6. c Arts et Métiers Institute of Technology MSMP HESAM Universite
Zehao Qin, Nan Kang, Huajing Zong, 等. Improved fatigue properties of laser powder bed fusion of Al–4.74Mg–0.70Sc–0.32Zr alloy via hot isostatic pressing[J]. 材料研究快报(英文), 2022,10(11):720-727.
Zehao Qin, Nan Kang, Huajing Zong, et al. Improved fatigue properties of laser powder bed fusion of Al–4.74Mg–0.70Sc–0.32Zr alloy via hot isostatic pressing[J]. Materials Research Letters, 2022, 10(11): 720-727.
Zehao Qin, Nan Kang, Huajing Zong, 等. Improved fatigue properties of laser powder bed fusion of Al–4.74Mg–0.70Sc–0.32Zr alloy via hot isostatic pressing[J]. 材料研究快报(英文), 2022,10(11):720-727.DOI: 10.1080/21663831.2022.2088252.
Zehao Qin, Nan Kang, Huajing Zong, et al. Improved fatigue properties of laser powder bed fusion of Al–4.74Mg–0.70Sc–0.32Zr alloy via hot isostatic pressing[J]. Materials Research Letters, 2022, 10(11): 720-727.DOI: 10.1080/21663831.2022.2088252.
Improved fatigue properties of laser powder bed fusion of Al–4.74Mg–0.70Sc–0.32Zr alloy via hot isostatic pressing
Laser powder bed fusion (L-PBF) processed components usually exhibit reduced fatigue performance owing to unavoidable defects at multiple scales
especially when the loading direction is parallel to the building direction. In this study
hot isostatic pressing (HIP) was applied to the L-PBFed Al-4.74Mg-0.70Sc-0.32Zr (wt.%) alloy to enhance the fatigue properties with a focus on the defect (porosities and inclusions) effects
compared with the direct-aged samples. The results demonstrated that HIP induced inconspicuous microstructural effects
but it healed the porosities and promoted oxidation. Therefore
the fatigue crack initiation transformed the oxide-associated porosity into an oxide